Video library

MIM Defect Investigation

Trace the symptom back through molding, debinding and sintering

Read the full article and infographic ยท CSMFG powder metallurgy services

Transcript

Start with the defect location

MIM defects can begin before they become visible. A crack found after sintering may have started during molding or handling.

Inspect earlier stages

Compare green, brown, and sintered parts. Trace the defect to the cavity, gate, core, ejector, and furnace support.

Cracks and incomplete filling

Review weld-line position, filling, venting, ejection, and handling. A repeated crack at one feature differs from random cracks across a batch.

Blisters and distortion

Binder-removal conditions, thick sections, segregation, and support can contribute. Use records and representative sections to narrow the cause.

Validate the correction

Run a controlled trial and check for new defects. Where integrity matters, use the agreed functional or material test as well as dimensions.

Keep traceable records

Connect feedstock, cavity, debinding, and furnace batches to inspection. Discuss the drawing and defect pattern with CSMFG.